- News
- Books
Featured Books
- pcb007 Magazine
Latest Issues
Current IssueThe Hole Truth: Via Integrity in an HDI World
From the drilled hole to registration across multiple sequential lamination cycles, to the quality of your copper plating, via reliability in an HDI world is becoming an ever-greater challenge. This month we look at “The Hole Truth,” from creating the “perfect” via to how you can assure via quality and reliability, the first time, every time.
In Pursuit of Perfection: Defect Reduction
For bare PCB board fabrication, defect reduction is a critical aspect of a company's bottom line profitability. In this issue, we examine how imaging, etching, and plating processes can provide information and insight into reducing defects and increasing yields.
Voices of the Industry
We take the pulse of the PCB industry by sharing insights from leading fabricators and suppliers in this month's issue. We've gathered their thoughts on the new U.S. administration, spending, the war in Ukraine, and their most pressing needs. It’s an eye-opening and enlightening look behind the curtain.
- Articles
- Columns
- Links
- Media kit
||| MENU - pcb007 Magazine
Catching Up (Literally) with Uyemura’s George Milad at SMTAI 2016
November 14, 2016 | Patty Goldman, I-Connect007Estimated reading time: 12 minutes

I managed to catch up with George Milad of Uyemura at the recent SMTA International conference, which wasn’t easy to do. But he did take a few minutes to fill me in on his schedule for the week and it certainly was packed, with a tutorial, presentations and IPC committee meetings.
Patty Goldman: Hi, George, it’s great to see you again—about twice a year, right? Let’s talk a little bit about what you’re presenting here at the SMTAI conference.
George Milad: I have had a very busy schedule. Yesterday I gave a presentation, a four-hour tutorial, and I will never do that again. To stand up and talk for four complete hours, it's very challenging staying alert and relevant and keeping the audience’s attention and making sure you're delivering value, because these people paid money to sit in that meeting. That was very challenging but it went very well and I'm happy. I get energized by the feedback from the attendees in the class, but then when I got back to my hotel, I was trying to listen to the presidential debate and I fell asleep after the first five minutes. (Laughs)
Goldman: I heard it was not that exciting of a debate, anyhow. But that does sound exhausting. How many people were in your audience?
Milad: We had approximately 15 people who signed up and paid money. That is very rewarding, because I gave the same training course at PCB West and I think if you signed up it was free, and I had three people show up. I talked forever for three people and it kills your energy, but this one was a very rewarding experience.
Goldman: You imparted a lot of knowledge.
Milad: Yes, they thought it was good. They filled in the forms and so I'll get some feedback from SMTA. Then first thing in the morning tomorrow I'm going to talk about the “Via Fill Copper Plating Process” and what it takes to optimize the via fill process. I-Connect007 published an article along these lines recently and this is basically the same concept but in the form of a presentation rather than an article.
Then I have the IPC 4-14 Plating Processes subcommittee meeting. Our committee meetings are not so critical because we do our work by conference call.
Goldman: Yes, I was very impressed when we talked about that before. I've been very impressed with how you guys conduct those meetings every…how many weeks?
Milad: Every other week.
Goldman: You get a lot accomplished that way.
Milad: Indeed. Then you set things in motion, and you say, "Okay, we need to just make a test vehicle (TV) ." Somebody manufactures it and then every couple of weeks we find out the status, and when the TV is complete, we send it out to people to plate it. Then we send it back out for evaluation We're always following these activities and evaluating results, and then we begin to write the specification and get interaction from people who sometimes like what's being written or some people take a strong objection to what's being written. And for good reason—I'm not saying they will just object for the sake of objecting.
For this, we were rewriting the ENIG spec. We wanted to set the upper limit for ENIG. It was written in 2002.
Goldman: That's a long time ago.
Milad: Yeah, 14 years later we're revising the specification. In 2002, we agreed that gold should be a minimum of two microinches. We did not put an upper limit, but we wrote that it should typically be 3−5 microinches. Typically, 3−5 is not the specification. Minimum of 2 microinches is the specification. Anybody who read the specification said the IPC calls for 3−5 μins, which was a horrible thing. We never called for 3−5 μins and it created a lot of problems.
Now, we’ve come back and we are redefining the gold thickness. We put the lower limit of 1.6 μins instead of two. Then, we wanted to put an upper limit. We tried very hard to pass 3.2 μins as the upper limit. We got a lot of resistance from manufacturers who do ENIG surface finish for the medical industry. They called for a minimum of 3.0 μins. They are the biggest printed circuit shop in the United States, I don't feel I should mention their name, but they said they have medical customers who will require a 3.0 μins minimum. We wanted to put 3.2 as the maximum, leaving no room at all to work between 3.0 and 3.2 μins. They kept arguing and finally we conceded and we put 4.0 μins as the upper limit. That is what the new specs will say, 1.6 to 4.0 μins. This is the first time we put an upper limit and as far as the 3−5 μins, we're hoping that will go by the wayside.
Goldman: I imagine it is a problem to put too much down, isn't it?
Milad: Absolutely. The problem with putting too much down is you're staying in the gold bath for a prolonged amount of time and that gives a lot of opportunity for nickel corrosion, or black pad. It's always been our objective to say, “Don't do that. You need only 2.0 μins. Get them deposited on the nickel and get out of the bath. There is no reason to stay any longer.”
It's not that it's guaranteed that if you stay longer in the bath that you're going to have corrosion, but if the nickel is a little bit compromised, it's not the perfect nickel, and you stay too long you will get corrosion. If you have the perfect nickel, it can withstand prolonged dwell in the gold bath, but nobody makes perfect nickel 100% of the time. We felt it's very important to restrict the gold thickness.
Goldman: This corrosion you're talking about is black pad, right?
Milad: Yes, the nickel corrosion and black pad are synonymous. If it is too extensive, then the pad is not going to solder, and the whole objective of the ENIG finish is that it’s a solderable finish. That's the story there. We don't want you to stay too long in the gold baths.
We also are including a corrosion chart in this new revision of the ENIG specification, which was quite challenging because when you have corrosion and you do a cross-section, it appears as spikes. When you look at a cross-section under 1000x magnification and you see less than 10 spikes in the field of view, that's acceptable. If you have more than 10 spikes, that's not acceptable. If the spikes are joined together, meaning they blend, one spike runs into the other, that's not acceptable. If the spike is too deep, that's not acceptable. We specified that and we ran into a huge tizzy of argumentation.
Is it 10? Is it 8? Is it 9? Is it 11? Is it 12? We finally said that we're just going to define what is acceptable and we're going to define what is rejectable. We're going to admit that there is a gray area between acceptable and rejectable.
Goldman: Yes, like saying 10 is good but 11 is bad? It seems that people might say, "Wait a minute. That's not that bad, is it?”
Milad: Yeah, so we decided to leave everything in between for the buyer and the manufacturer to sort out. If it's less than 10, we don't want any argument. We want this to be acceptable.
Page 1 of 2
Suggested Items
Driving Innovation: Direct Imaging vs. Conventional Exposure
07/01/2025 | Simon Khesin -- Column: Driving InnovationMy first camera used Kodak film. I even experimented with developing photos in the bathroom, though I usually dropped the film off at a Kodak center and received the prints two weeks later, only to discover that some images were out of focus or poorly framed. Today, every smartphone contains a high-quality camera capable of producing stunning images instantly.
Hands-On Demos Now Available for Apollo Seiko’s EF and AF Selective Soldering Lines
06/30/2025 | Apollo SeikoApollo Seiko, a leading innovator in soldering technology, is excited to spotlight its expanded lineup of EF and AF Series Selective Soldering Systems, now available for live demonstrations in its newly dedicated demo room.
Indium Corporation Expert to Present on Automotive and Industrial Solder Bonding Solutions at Global Electronics Association Workshop
06/26/2025 | IndiumIndium Corporation Principal Engineer, Advanced Materials, Andy Mackie, Ph.D., MSc, will deliver a technical presentation on innovative solder bonding solutions for automotive and industrial applications at the Global Electronics A
Fresh PCB Concepts: Assembly Challenges with Micro Components and Standard Solder Mask Practices
06/26/2025 | Team NCAB -- Column: Fresh PCB ConceptsMicro components have redefined what is possible in PCB design. With package sizes like 01005 and 0201 becoming more common in high-density layouts, designers are now expected to pack more performance into smaller spaces than ever before. While these advancements support miniaturization and functionality, they introduce new assembly challenges, particularly with traditional solder mask and legend application processes.
Knocking Down the Bone Pile: Tin Whisker Mitigation in Aerospace Applications, Part 3
06/25/2025 | Nash Bell -- Column: Knocking Down the Bone PileTin whiskers are slender, hair-like metallic growths that can develop on the surface of tin-plated electronic components. Typically measuring a few micrometers in diameter and growing several millimeters in length, they form through an electrochemical process influenced by environmental factors such as temperature variations, mechanical or compressive stress, and the aging of solder alloys.