Advanced Atomic Layer Deposition Enables Lithium-Ion Battery Technology
May 9, 2017 | NRELEstimated reading time: 2 minutes
The U.S. Department of Energy's National Renewable Energy Laboratory (NREL) has entered into an exclusive license agreement with Forge Nano to commercialize NREL's patented battery materials and systems capable of operating safely in high-stress environments. A particular feature of the technology is the encapsulation of materials with solid electrolyte coatings that can be designed to meet the increasingly demanding needs of any battery application.
These lithium-ion batteries feature a hybrid solid-liquid electrolyte system, in which the electrodes are coated with a solid electrolyte layer. This layer minimizes the potential for the formation of an internal short circuit between electrodes to prevent "thermal runaway," or the uncontrolled increase in battery cell temperature that can result in a fire or an explosion.
In addition, coating of the electrode materials reduces the stress on traditional polymer separators that are currently necessary components in commercial lithium-ion batteries and can allow for thinner separators designed for higher power devices. This advancement has the potential to reduce both the cost and weight of the battery device, while substantially increasing safety and lifetime.
Lab-scale testing of NREL's hybrid solid-liquid electrolyte system has shown increased electrode durability and reliability without compromised electrochemical performance. "The cells are less likely to fail, even in demanding, real-world conditions like high temperatures and fast recycle rates," said Ahmad Pesaran, whose team of engineers in NREL's Energy Storage group invented the technology.
Forge Nano, formerly PneumatiCoat Technologies, is a Colorado-based company specializing in the scale-up and manufacturing of cost-effective Atomic Layer Deposition (ALD) encapsulated materials. Forge Nano presented its technology at the 2013 and 2017 NREL Industry Growth Forum, the nation's premier clean energy investment event. A year later, NREL approached the company as a potential licensee after conducting a licensee search in the battery technology area.
"This license agreement will allow Forge Nano to offer further customized lithium-ion battery materials for high performance devices by utilizing our patented high-throughput ALD system that has already been successfully tested at the pilot scale and in large format pouch cells," Paul Lichty, CEO of Forge Nano, said. "The incorporation of this technology into Forge Nano's offering will lead to a substantial reduction in cost per unit energy of lithium-ion batteries."
NREL has more than 800 technologies available for licensing. Companies interested in partnering to advance research on or commercialize renewable energy technologies can visit the EERE Energy Innovation Portal, which features descriptions of all renewable energy technologies funded by the Department of Energy's Office of Energy Efficiency and Renewable Energy.
NREL is the U.S. Department of Energy's primary national laboratory for renewable energy and energy efficiency research and development. NREL is operated for the Energy Department by The Alliance for Sustainable Energy, LLC.
For more information click here.
Suggested Items
Indium Experts to Present on High-Temperature, Lead-Free Solder Paste and High Reliability Liquid Metal Alloys Poster at ECTC
05/16/2024 | Indium CorporationIndium Corporation Research Associate Kyle Aserian will deliver a presentation at the 74th Electronic Components and Technology Conference (ECTC) on May 31, in Denver, Colorado.
Siemens, Foxconn Team Up to Optimize Forward-thinking Manufacturing
05/16/2024 | FoxconnSiemens AG, a leading technology company, and Hon Hai Technology Group (Foxconn), the world’s largest electronics manufacturer, have signed a memorandum of understanding (MoU) to drive digital transformation and sustainability in smart manufacturing platforms.
TactoTek Licenses IMSE Technology to Polestar for Sustainable Electronics Design Innovation
05/15/2024 | TactoTekPolestar, the Swedish electric performance car brand, and Finnish smart surface pioneer TactoTek, have entered a collaboration to explore integration of Injection Molded Structural Electronics (IMSE) technology into Polestar’s vehicle programs.
SiPearl: Partnership with Samsung Electronics for built-in HBM in Rhea
05/14/2024 | BUSINESS WIRESiPearl, the company building the high-performance low-power European microprocessor for HPC and AI inference, has signed a partnership with Samsung Electronics Co. Ltd., a world leader in advanced memory technology, to equip its Rhea series with Samsung’s advanced memory solution ideal for HPC and AI applications.
ispace EUROPE, CDS Sign Payload Service Agreement to Transport Precise Location Measurement Technology to the Moon
05/14/2024 | BUSINESS WIREispace EUROPE S.A., the Luxembourg-based subsidiary of ispace, inc., and Control Data Systems SRL (CDS) have signed a payload services agreement to transport precise location measurement equipment to the Moon, the two companies announced.