- News
- Books
Featured Books
- smt007 Magazine
Latest Issues
Current IssueWhat's Your Sweet Spot?
Are you in a niche that’s growing or shrinking? Is it time to reassess and refocus? We spotlight companies thriving by redefining or reinforcing their niche. What are their insights?
Moving Forward With Confidence
In this issue, we focus on sales and quoting, workforce training, new IPC leadership in the U.S. and Canada, the effects of tariffs, CFX standards, and much more—all designed to provide perspective as you move through the cloud bank of today's shifting economic market.
Intelligent Test and Inspection
Are you ready to explore the cutting-edge advancements shaping the electronics manufacturing industry? The May 2025 issue of SMT007 Magazine is packed with insights, innovations, and expert perspectives that you won’t want to miss.
- Articles
- Columns
- Links
- Media kit
||| MENU - smt007 Magazine
Approaches to Overcome Nodules and Scratches on Wire-Bondable Plating on PCBs
July 17, 2019 | Young K. Song and Vanja Bukva, Teledyne Dalsa Inc., and Ryan Wong, FTG CircuitsEstimated reading time: 4 minutes

Abstract
Initially adopted internal specifications for acceptance of printed circuit boards (PCBs) used for wire bonding was that there were no nodules or scratches allowed on the wirebond pads when inspected under 20X magnification. The nodules and scratches were not defined by measurable dimensions and were considered to be unacceptable if there was any sign of a visual blemish on wire-bondable features. Analysis of the yield at a PCB manufacturer monitored monthly for over two years indicated that the target yield could not be achieved, and the main reasons for yield loss were due to nodules and scratches on the wirebonding pads.
The PCB manufacturer attempted to eliminate nodules and scratches. First, a light-scrubbing step was added after electroless copper plating to remove any co-deposited fine particles that acted as a seed for nodules at the time of copper plating. Then, the electrolytic copper plating tank was emptied, fully cleaned, and filtered to eliminate the possibility of co-deposited particles in the electroplating process. Both actions greatly reduced the density of the nodules but did not fully eliminate them. Even though there was only one nodule on any wire-bonding pad, the board was still considered a reject. To reduce scratches on wirebonding pads, the PCB manufacturer utilized foam trays after routing the boards so that they did not make direct contact with other boards. This action significantly reduced the scratches on wire-bonding pads, even though some isolated scratches still appeared from time to time, which caused the boards to be rejected. Even with these significant improvements, the target yield remained unachievable.
Another approach was then taken to consider if wire bonding could be successfully performed over nodules and scratches and if there was a dimensional threshold where wire bonding could be successful. A gold ball bonding process called either stand-off-stitch bonding (SSB) or ball-stitch-on-ball bonding (BSOB) was used to determine the effects of nodules and scratches on wire bonds. The dimension of nodules, including height, and the size of scratches, including width, were measured before wire bonding. Wire bonding was then performed directly on various sizes of nodules and scratches on the bonding pad, and the evaluation of wire bonds was conducted using wire pull tests before and after reliability testing. Based on the results of the wire-bonding evaluation, the internal specification for nodules and scratches for wirebondable PCBs was modified to allow nodules and scratches with a certain height and a width limitation compared to initially adopted internal specifications of no nodules and no scratches. Such an approach resulted in improved yield at the PCB manufacturer.
Introduction
The development of the chip-on-board (COB) type of image sensors has significantly increased in the last few years to accommodate an increasing demand for low-cost, high-performance industrial inspection cameras. Wire bonding is the most commonly used technology for making the electrical interconnection between a silicon image sensor and its substrate during image sensor fabrication. Therefore, wire bonding directly on the PCB surface is inevitable for COB-type image sensor fabrication.
IPC-A-600J section 2.7.1.3—surface plating, wire-bond pads [1]—states, “Wire-bond pads are free of surface nodules, roughness, electrical test witness marks or scratches that exceed 0.8 mm (32 min) RMS (root-mean-square) in the pristine area in accordance with an applicable test method AABUS.” Since the tolerance of surface nodules (<0.8 mm RMS) in IPC-A-600J for wire bonding pads is not easily measurable and may not properly reflect single nodules and shallow scratches, the initially adopted specification for wire bonding pads as a user was defined to be free of surface nodules and scratches.
Figure 1: Average yield loss from multiple wire-bonding PCB products.
Therefore, a board was considered a reject if a nodule or a scratch was visible in the pristine area of the wire-bond at 20X magnification. If in any doubt, one could use 40X magnification for inspection to clarify pass/fail. However, in reality, it was difficult to achieve a wire-bonding surface in specification without nodules or scratches, resulting in low yield at the PCB manufacturer. In particular, PCB products designed with a center cut-out slot close to bonding pads were prone to significant yield loss due to nodules.
Yield review with the manufacturer and the analysis of causes for rejects using Pareto charts pointed out that two main reasons for PCB rejects were due to nodules and scratches on the wire-bonding surface. Yield had been reviewed on a monthly basis for 28 months, and the major yield losses continued to be due to nodules and scratches on the wire-bonding surface during the period. Figure 1 shows the average yield loss per month for wire-bonding boards due to nodules and scratches. The average yield losses from multiple PCB products due to nodules and scratches for wire bonding boards were in the range of 4–41% and 2–30%, respectively, during the period.
It is worth noting that the data in Figure 1 may not necessarily provide the picture of actual average yield loss due to nodules and scratches. When any defect—either nodule or scratch—was first found during an inspection of a board, the reason for rejection was recorded and further inspection of that board was not pursued since the board was already determined to be a reject. For example, the manufacturer recorded a 39% yield loss for nodules and none for scratches in Period 3. However, it may not mean that there were no scratches on those rejected boards since those boards had not been inspected further for scratches after nodules were first observed.
To read the full article, which appeared in the July 2019 issue of SMT007 Magazine, click here.
Suggested Items
The Evolution of Picosecond Laser Drilling
06/19/2025 | Marcy LaRont, PCB007 MagazineIs it hard to imagine a single laser pulse reduced not only from nanoseconds to picoseconds in its pulse duration, but even to femtoseconds? Well, buckle up because it seems we are there. In this interview, Dr. Stefan Rung, technical director of laser machines at Schmoll Maschinen GmbH, traces the technology trajectory of the laser drill from the CO2 laser to cutting-edge picosecond and hybrid laser drilling systems, highlighting the benefits and limitations of each method, and demonstrating how laser innovations are shaping the future of PCB fabrication.
Day 2: More Cutting-edge Insights at the EIPC Summer Conference
06/18/2025 | Pete Starkey, I-Connect007The European Institute for the PCB Community (EIPC) summer conference took place this year in Edinburgh, Scotland, June 3-4. This is the third of three articles on the conference. The other two cover Day 1’s sessions and the opening keynote speech. Below is a recap of the second day’s sessions.
Day 1: Cutting Edge Insights at the EIPC Summer Conference
06/17/2025 | Pete Starkey, I-Connect007The European Institute for the PCB Community (EIPC) Summer Conference took place this year in Edinburgh, Scotland, June 3-4. This is the second of three articles on the conference. The other two cover the keynote speeches and Day 2 of the technical conference. Below is a recap of the first day’s sessions.
Preventing Surface Prep Defects and Ensuring Reliability
06/10/2025 | Marcy LaRont, PCB007 MagazineIn printed circuit board (PCB) fabrication, surface preparation is a critical process that ensures strong adhesion, reliable plating, and long-term product performance. Without proper surface treatment, manufacturers may encounter defects such as delamination, poor solder mask adhesion, and plating failures. This article examines key surface preparation techniques, common defects resulting from improper processes, and real-world case studies that illustrate best practices.
RF PCB Design Tips and Tricks
05/08/2025 | Cherie Litson, EPTAC MIT CID/CID+There are many great books, videos, and information online about designing PCBs for RF circuits. A few of my favorite RF sources are Hans Rosenberg, Stephen Chavez, and Rick Hartley, but there are many more. These PCB design engineers have a very good perspective on what it takes to take an RF design from schematic concept to PCB layout.