Nihon Superior Co. Ltd., an advanced joining material supplier, will exhibit in Booth 1325 during the 2024 IPC APEX EXPO, scheduled to take place April 9-11, 2024 at the Anaheim Convention Center in California. Renowned for its commitment to innovation, Nihon Superior will present a range of groundbreaking products, including the SN100CV® P608 solder paste and the TempSave™ series of low-temperature soldering materials.
SN100CV® P608 sets a new standard as a completely halogen-free, lead-free, and no-clean solder paste by Nihon Superior. In contrast to silver-containing alloys relying on a dispersion of fine particles of eutectic Ag3Sn for strength, SN100CV achieves its robustness from solute atoms within the tin matrix of the joint. Remarkably, in tensile tests, SN100CV matches the strength of SAC305 while retaining a high resistance to impact loading, offering exceptional performance in various applications.
For high-reliability applications demanding strength surpassing SAC305, Nihon Superior introduces the LF-C2 lead-free alloy. Leveraging both dispersion and solid solution strengthening, LF-C2 delivers superior strength. With a liquidus temperature of 213°C, it facilitates reflow at a lower temperature than SAC305.
The P608 flux medium ensures wetting comparable to halogen-containing pastes, despite being completely halogen-free. SN100CV P608 and LF-C2 exhibit outstanding performance across diverse component types and process parameters.
Additionally, Nihon Superior presents the TempSave™ series of low-temperature soldering materials, addressing industry goals such as reducing peak reflow temperature, minimizing package warpage, lowering energy consumption during reflow, and protecting temperature-sensitive devices.
- TempSave B58: A eutectic SnBi alloy with a low melting point of 139°C.
- TempSave B37: A ductile hypoeutectic SnBi alloy without Ag, offering exceptional drop performance, surpassing SAC305. The P610 flux medium, specifically designed for Bi alloys, ensures halogen-free compatibility. The TempSave B37 P610 solder paste can be reflowed with a peak temperature of 190°C. Additionally, a high-speed jetting paste version, TempSave B37 P611, provides consistent dot sizes.
Visit Booth 1325 at the 2024 IPC APEX EXPO to explore Nihon Superior's latest alloys, solder pastes, and lead-free products.
Suggested Items
Book Excerpt: The Printed Circuit Assembler’s Guide to... Low-Temperature Soldering, Vol. 2, Chapter 5
12/23/2024 | I-Connect007 Editorial TeamChapter 5 introduces the advantages of using low-temperature soldering for through-hole components, including cost efficiency, reliability improvement, and reduced warpage. Also covered: the evaluation of different fluxes and the performance of HRL3 in wave soldering and selective soldering processes.
PDR Offers Advanced Infrared Heating Technology for BGA Rework
12/02/2024 | PDRPDR Americas is proud to highlight its industry-leading solutions for BGA and SMT rework. As a trusted partner in electronics manufacturing, PDR’s rework stations deliver precision, reliability, and simplicity, setting a new standard for addressing the challenges of modern rework applications.
sureCore Now Licensing its CryoMem Range of IP for Quantum Computing
11/26/2024 | sureCoresureCore, the memory specialist, has announced that it is now licensing its CryoMem™ suite of Memory IP that is designed for use at the extremely low temperatures required for Quantum Computing (QC) applications.
Indium Technical Expert to Present at SiP Conference China
11/25/2024 | Indium CorporationIndium Corporation Senior Area Technical Manager for East China Leo Hu is scheduled to deliver a presentation on Low-Temperature Solder Material in Semiconductor Packaging Applications at SiP China Conference 2024 on November 27 in Suzhou, China.
DELO Introduces UV-approach for Fan-out Wafer-level Packaging
10/25/2024 | DELODELO has developed a new approach for fan-out wafer-level packaging (FOWLP). Its feasibility study shows: With the use of UV-curable molding materials instead of heat curing ones, warpage and die shift can be reduced significantly. Additionally, this leads to improvements in curing time and minimizes the energy consumption.