- News
- Books
Featured Books
- pcb007 Magazine
Latest Issues
Current IssueThe Hole Truth: Via Integrity in an HDI World
From the drilled hole to registration across multiple sequential lamination cycles, to the quality of your copper plating, via reliability in an HDI world is becoming an ever-greater challenge. This month we look at “The Hole Truth,” from creating the “perfect” via to how you can assure via quality and reliability, the first time, every time.
In Pursuit of Perfection: Defect Reduction
For bare PCB board fabrication, defect reduction is a critical aspect of a company's bottom line profitability. In this issue, we examine how imaging, etching, and plating processes can provide information and insight into reducing defects and increasing yields.
Voices of the Industry
We take the pulse of the PCB industry by sharing insights from leading fabricators and suppliers in this month's issue. We've gathered their thoughts on the new U.S. administration, spending, the war in Ukraine, and their most pressing needs. It’s an eye-opening and enlightening look behind the curtain.
- Articles
- Columns
- Links
- Media kit
||| MENU - pcb007 Magazine
Estimated reading time: 1 minute

Let's Talk Testing: Seeing is Believing in Fractographic Analysis
One of the more common types of failure analysis is the investigation of something that has broken. For this column, we will be discussing a broken material, or, more commonly, a fractured or cracked material.
Fractographic analysis is sometimes perceived as a difficult analysis, given its roots in material science, but one might be surprised to learn that failure modes for this type of study are well-established and well reported and can easily be found in textbooks, reference materials, and even with a Google search! Given that, this column is not being written to teach a lesson in fractographic failure modes, but more so to provide some insight in performing the analysis yourself, or at least give you some direction to get things started.
Unlike many types of forensic analyses, a fractographic investigation most times doesn’t really need any high dollar, sophisticated instrumentation or equipment. This is true because the most pertinent information in a fracture based investigation is simply the visual examination of the fracture surface itself. Now, that can be problematic in some instances, because the fractured surface can become damaged before it is discovered. If a crack happens and is still connected on one end, it’s possible that the opposing surfaces of the fracture can make contact with each other—through movement of the specimen while still in use or even through simple vibration—potentially damaging the surface characteristics that are needed to determine the failure mode at hand. This is not overly common, but can happen, and as such it’s worth mentioning here. For this reason, one recommendation that can be made is…don’t put the pieces back together! In line with what has been mentioned just a few sentences ago, putting the fractured pieces back together can accidentally damage what you’re really trying to inspect.
Editor's Note: This column originally appeared in the July 2016 issue of The PCB Magazine. This is Keith’s first in a series of columns having to do with inspection and test— from the test lab perspective.
More Columns from Let's Talk Testing
Let’s Talk Testing: Professor Plum in the Library with the Candlestick…Right?Random Thoughts on Employment, from Both Sides of the Table…
Let's Talk Testing: You’re in for a (Thermal) Shock!
Let's Talk Testing: How Strong is Your Foundation?
Got Whiskers?
Let's Talk Testing: Are You Getting What You’ve Asked for?
Vias for Dummies
Don’t Reinvent the Wheel—Find an Expert!